Wood-Polymer Bonding in Extruded and Nonwoven Web Composite Panels
Technical paper comparing the effectiveness of a maleated polypropylene (MAPP) as a coupling agent in extruded wood flour/polypropylene composites, and nonwoven web wood fiber/polypropylene composites. Authors: Andrzej M. Krzysik and others.
No queries for www.fpl.fs.fed.us/documnts/pdf1991/krzys91a.pdf