Mechanical Holding Power of Melt-Blend Boards Made from Recycled Plastic and Kenaf
Technical paper presenting the progress of an on-going research project to demonstrate the viability of using agricultural fibers and recycled plastics in producing thermoplastic composites. Authors: P. Chow and others.
|