Combining Cellulose Fiber and Wollastonite Mineral Fibers into a Nylon-6 Matrix
Technical paper about research aimed at developing a high purity cellulose/wollastonite pellet which can be accurately metered and fed into a laboratory scale twin-screw extruder and compounded with nylon-6 resing to create hybrid composites. Authors: R.E. Jacobson and D.F. Caulfield.