Weathering Characteristics of Fiber-Plastic Composites
Technical paper presented at the fifth International Conference on Woodfiber-Plastic Composites, summarising a 2-year testing program designed to assess the environmental degradation of wheat straw-filled polypropylene and polyethylene composites. Authors: Donna A. Johnson
|